[Use Case] Preventing scrap generation during press processing
A case where wear resistance and seizure resistance were improved through the coating treatment of die punches!
We would like to introduce examples of applications for the discharge coating and buildup device "Depo Series." By coating tungsten carbide on dies and punches, wear resistance and seizure resistance are provided, preventing the lifting of the knockout plate when ejecting the punch and preventing crimping. This is particularly effective for sticky materials such as stainless steel and aluminum. [Factors and Issues Causing Scrap in Press Processing] ■ Adhesion due to vacuum ■ Adhesion to punch cutting edges caused by scrap return, etc. ■ Adhesion due to oil film ■ Adhesion due to punch magnetism (residual magnetism) ■ Lifting caused by compressed air in the die *For more details, please refer to the PDF document or feel free to contact us.